How to Prepare Tungsten Disulfide Nanosheet?
- Details
- Category: Tungsten Information
- Published on Monday, 25 May 2020 13:52
How to prepare tungsten disulfide nanosheet? It is reported that tungsten disulfide (WS2) nanosheet powder can be prepared by mechanical peeling.
More details, please visit:
http://tungsten-disulfide.com/index.html
Preparation of Tungsten Disulfide Nanosheets
Disperse the bulk commercial tungsten disulfide powder in 2-methylpyrrolidone at a feed liquid ratio of 1-2 mg/mL to obtain a dispersion of tungsten disulfide powder. Place the dispersion in a cell crusher and continue to crush for 20-40 min. After standing for 15-30 minutes, the solid was obtained after centrifugation, washed with ethanol for several times and then dried to obtain tungsten disulfide nanosheets. The obtained WS2 nanosheets have excellent optical properties, high corrosion resistance and structural stability, and are mainly used to fabricate a catalytic anode in a visible light-responsive low-temperature fuel cell.
ChinaTungsten Online has more than 23 years of experience in research, development, production and sales of tungsten chemicals. We can provide you with high-quality tungsten disulfide powder at competitive prices. And there are different specifications for you to choose.
- Tungsten Oxide Manufacturer & Supplier, Chinatungsten Online: www.tungsten-oxide.com
- Tungsten News & Prices of China Tungsten Industry Association: www.ctia.com.cn
- Molybdenum News & Price: news.molybdenum.com.cn
- Tel.: 86 592 5129696; Fax: 86 592 5129797; Email: sales@chinatungsten.com