How to prepare high purity ammonium paratungstate? The researchers proposed an economical method for preparing high purity ammonium paratungstate with high yield and simple process.
More details, please visit:
http://ammonium-paratungstate.com/index.html
A Preparation Method of High Purity Ammonium Paratungstate
Pour 215 L of deionized water in a heated 200 L stirred reactor. Add 200 kg of APT·10H2O with stirring. Then, the suspension was treated at 90 °C for 2 h with stirring. When the molar ratio of NH3: W is 0.77: 1, the NH3 concentration in the liquid phase is 2.1 g/L. The pH at room temperature is 6.8. The mass ratio of solid to aqueous solution is 0.80: 1. After the treatment, the suspension was filtered, the product was washed with 10 L of deionized water, and finally dried at 100 °C to obtain 184 kg (corresponding to a yield of 95.3%) of high purity ammonium paratungstate.
- APT Manufacturer & Supplier, Chinatungsten Online: ammonium-paratungstate.com
- Tungsten News & Prices of China Tungsten Industry Association: www.ctia.com.cn
- Molybdenum News & Price: news.molybdenum.com.cn
- Tel.: 86 592 5129696; Fax: 86 592 5129797; Email: sales@chinatungsten.com