A Tungsten Tailings Recovery Process From Low-grade Tungsten

The present invention relates to a process for recovering tungsten from low grade tungsten-containing tailing process, the technical field belonging to a wet extraction from the group of metal compounds in the ore or concentrate. Tungsten recovery process includes a buffer pool classification, flannel chute roughing, roughing shaker, yurts selection and shaker sweep the election process. Supporting the selection of the buffer pool 2, flannel chute 10 to 15, yurts from 2 to 4, Shaker 10 to 15 units. The mass percent of the treated low-grade tungsten-containing tailings W03 is 0.04 to 0.08%. Through the recovery of low-grade tungsten tailings, get a good grade and recovery, to increase the economic benefits of selected plants, but also to achieve the comprehensive utilization of resources.


Tungsten Manufacturer & Supplier: Chinatungsten Online - http://www.chinatungsten.com
Tel.: 86 592 5129696; Fax: 86 592 5129797
Email:   sales@chinatungsten.com
Tungsten News & Tungsten Prices, 3G Version: http://3g.chinatungsten.com
Tungsten News & Tungsten Prices, WML Version: http://m.chinatungsten.com

The above is reproduced from: Application Technology Network, if in doubt, please contact the content belongs website.

 

 

WeChat