The Recycling of Tungsten Carbide

Brief description of this technology:  
The present invention relates to the method of containing iron or tungsten powder or the powder aggregation .This invenition includes  these following steps:


碳化钨
At the begining,  we can mix powder containing tungsten carbide at least one first powder level with powder containing the iron oxide or tungsten oxide-containing powder and  any kind of  iron powder of at least a second powder fraction mixed ( The weight of the first fraction is 50-90% of the weight of the mixture,the weight of the second fraction is 10-50% of the weight of the mixture.)

The heating step  is the second step.
The mixture should be heated up to 400-1300 ° C. The perferred temperature of the mixture is 1000-1200 ℃. The present invention also relates to the iron powder,
tungsten powder and power aggregates.



Tungsten Manufacturer & Supplier: Chinatungsten Online - http://www.chinatungsten.com
Tel.: 86 592 5129696; Fax: 86 592 5129797
Email: sales@chinatungsten.com
Tungsten News & Tungsten Prices, 3G Version: http://3g.chinatungsten.com
Tungsten News & Tungsten Prices, WML Version: http://m.chinatungsten.com

 

 

WeChat