Preparation of Nano Violet Tungsten Oxide
- Details
- Category: Tungsten Information
- Published on Friday, 15 November 2019 19:08
- Written by Yanqiu
- Hits: 1864

Nano violet tungsten oxide with strong light absorbing ability can be used as photothermal conversion material. It has high application value in the treatment of cancer. As for its preparation, tungsten source and organic solvents are used as raw materials.
Nano Violet Tungsten Oxide Used in Cancer Treatment
- Details
- Category: Tungsten Information
- Published on Friday, 15 November 2019 19:03
- Written by Yanqiu
- Hits: 1840

Nano violet tungsten oxide has strong absorbing ability of near-infrared light. Therefore, it can be used as a kind of photothermal conversion material. And it has high application value in cancer treatment.
Read more: Nano Violet Tungsten Oxide Used in Cancer Treatment
Ultrafine W18O49 Nanowire Prepared by Solvothermal Method
- Details
- Category: Tungsten Information
- Published on Thursday, 14 November 2019 20:34
- Written by Yanqiu
- Hits: 1883

As a kind of multi-functional material, ultrafine W18O49 nanowire has high application value in many important fields, such as gas-sensing materials, sensors and photodetectors. It is usually prepared by solvothermal method, which is simple and environmentally friendly.
Read more: Ultrafine W18O49 Nanowire Prepared by Solvothermal Method
How to Prepare Nano Violet Tungsten Oxide?
- Details
- Category: Tungsten Information
- Published on Thursday, 14 November 2019 20:38
- Written by Yanqiu
- Hits: 1968

Nano violet tungsten oxide (WO2.72) with size less than 10 nm can be synthesized by alcoholysis and heat treatment. Compared with other forms, nano-sized violet tungsten oxide has better photocatalytic performance. It is a kind of photocatalysis material with high efficiency.
How to Prepare Ultrafine W18O49 Nanowire?
- Details
- Category: Tungsten Information
- Published on Thursday, 14 November 2019 20:32
- Written by Yanqiu
- Hits: 1813

Ultrafine W18O49 nanowire is prepared by WCl6 and triethylene glycol. During the preparation process, WCl6 is used as precursor, and triethylene glycol is used as solvent. This is an efficient and environmentally friendly preparation method.