4.Proper operation process. For the pheumatic spray drying tower, the process parameter often refers to drying temperature, feeding velocity and pressure of nozzle. Drying temperature includes inlet air temperature and outlet air temperature. Increase inlet air temperature can promote liquid evaporation, which will solidify the liquid before it contacts the wall which will reduce the wall sticking waste rate and increase yield of product. Besides that, temperature also affects the diameter of grains. When the temperature is low, the grain size is bigger which will prolong the drying process. When the inlet air temperature stay the same, raise the outlet air temperature can reduce the temperature differences to fasten drying efficiency.

5.The movement of hot air in the dry tower. The movement of hot air in the dry tower affects wall sticking directly. When the total amount of inlet air stay the same, the proportion of the air for protection atmosphere and air for drying will affects the drying result. If the air is insufficient for drying, liquid will stick on the wall before getting dried.



Tungsten Powder Manufacturer & Supplier: Chinatungsten Online - www.tungsten-powder.com
Tel.: 86 592 5129696; Fax: 86 592 5129797
Email: sales@chinatungsten.com
Tungsten & Molybdenum Information Bank: http://i.chinatungsten.com
Tungsten News & Tungsten Prices, 3G Version: http://3g.chinatungsten.com
Molybdenum News & Molybdenum Price: http://news.molybdenum.com.cn

 

 

 

 

WeChat