Tungsten Carbide Screw-tap’ Tapping Problem and Solution II
- Details
- Category: Tungsten Information
- Published on Friday, 18 July 2014 17:50
Some problems often occur when the tungsten carbide screw-tap’s is tapping, involving the high surface roughness of the inner thread. There are several factors and solutions in the followings:
1.Tungsten carbide screw-tap’s selection is incorrect; Choosing the right conditions to be processed by the tungsten carbide screw-tap.
2.Cutting speed is too high; Reduce cutting speed.
3.Cutting Cone length is not enough; Increase the length of the cutting cone.
4.Chip poor; Choosing the right conditions to be processed by the tungsten carbide screw-tap.
5.Bottom diameter is too small; Select the bottom hole diameter according to the corresponding standards.
6.Cold welding; Improve the cooling and lubrication conditions.
Tungsten Manufacturer & Supplier: Chinatungsten Online - http://www.chinatungsten.com
Tel.: 86 592 5129696; Fax: 86 592 5129797
Email: sales@chinatungsten.com
Tungsten & Molybdenum Information Bank: http://i.chinatungsten.com
Tungsten News & Tungsten Prices, 3G Version: http://3g.chinatungsten.com
Molybdenum News & Molybdenum Price: http://news.molybdenum.com.cn