Ammonium Metatungstate Preparing Ammonium Tetrathiotungstate
- Details
- Category: Ammonium Metatungstate
- Published on Wednesday, 02 November 2016 10:51
- Written by chunyan
- Hits: 1968

For shortening the reaction time, reducing pollution to the environment, and obtaining high purity product at the same time, an invention has pointed a method to prepare ammonium tetrathiotungstate from raw materials of ammonium metatungstate (AMT), concentrated ammonia water and ammonium sulfide solution, the steps are shown as following:
1. Weight a certain amount of ammonium metatungstate powder and add distilled water, control the ratio of dosage distilled water and AMT at among 3 ~ 6/1 (Calculated by ml/g);
2. Add a certain amount of concentrated ammonia water with stirring and heating to 40~60℃ to dissolve, the ratio of dosage concentrated ammonia water and AMT is 1~2/1 calculated by ml/g;
3. Control the solution temperature among the room temperature (25℃) to 90℃, then add ammonium sulfide solution with sulfur content of 6~12% with stirring, the mole ratio of sulfur and tungsten in the added amount of ammonium sulfide solution and reactant liquid is 4~6 to 1, and stir for 0.5~3 hours to get blood red liquid;
4. After the reaction finished, take out the reactant to cool to room temperature and get it crystallize for 8~24 hours, then filter the solution with crystal and wash them with cold distilled water for 3 times, finally wash the crystal with anhydrous ethanol for 2~3 times, then carry out drying solvent, drying under room temperature for 24 hours to get dark red needle crystal of ammonium tetrathiotungstate.
AMT Supplier: Chinatungsten Online ammonium-metatungstate.com | Tel.: 86 592 5129696; Fax: 86 592 5129797;Email:sales@chinatungsten.com |
Tungsten News&Tungsten Prices, 3G Version: http://3g.chinatungsten.com | Molybdenum News & Molybdenum Price: http://news.molybdenum.com.cn |