Non-sag Tungsten at Room Temperature Performance
- Details
- Category: Tungsten Information
- Published on Wednesday, 03 June 2015 17:53
- Written by Yahong
- Hits: 420
Non-sag tungsten wire shows its performance on wire winding performance at room temperature performance.
Because of its long processing flow, if the process is mismanaged, it is very easy to produce a lot of tiny cracks or will lead to local brittle, so when reeling it will easily break. Since the crack caused by the fracture was about to be hairy wire breakage, because the wire becomes brittle and fracture caused by flash-like crystal plane is rendered.
Tungsten Metals Manufacturer & Supplier: Chinatungsten Online - http://www.tungsten.com.cn
Tel.: 86 592 5129696; Fax: 86 592 5129797
Email: sales@chinatungsten.com
Tungsten & Molybdenum Information Bank: http://i.chinatungsten.com
Tungsten News & Tungsten Prices, 3G Version: http://3g.chinatungsten.com
Molybdenum News & Molybdenum Price: http://news.molybdenum.com.cn