Preparation Method for Tungsten Disulfide

The invention relates to the technical field of compound preparation and in particular to a preparation method for tungsten disulfide.

The preparation method comprises the following steps: uniformly mixing tungstic acid with an ammonium trisulfide solution to obtain a mixture; putting the mixture into vulcanization equipment, vacuumizing, and heating in the vulcanization equipment at first stage for 50-70 minutes at the temperature of 650-750 DEG C; heating at second stage for 110-130 minutes at the temperature of 1350-1400 DEG C to obtain tungsten disulfide. According to the preparation method, the process is short, the used equipment is simple, and the environmental pollution is alleviated at the same time.


Tungsten Manufacturer & Supplier: Chinatungsten Online - http://www.chinatungsten.com
Tel.: 86 592 5129696; Fax: 86 592 5129797
Email:   sales@chinatungsten.com
Tungsten News & Tungsten Prices, 3G Version: http://3g.chinatungsten.com
Tungsten News & Tungsten Prices, WML Version: http://m.chinatungsten.com

The above is reproduced from: Application Technology Network, if in doubt, please contact the content belongs website.

 

 

WeChat