From Tungsten Electrode to GTAW QualityⅡ

The article is the other part of GTAW quality on tungsten electrode, for example, the level of heat input impact on weld quality.

The level of heat input also affects weld quality. Low heat input, caused by low welding current or high welding speed, can limit penetration and cause the weld bead to lift away from the surface being welded. If there is too much heat input, however, the weld bead grows in width while the likelihood of excessive penetration and spatter increase. Additionally, if the welding torch is too far from the workpiece the shielding gas becomes ineffective, causing porosity within the weld. This results in a weld with pinholes, which is weaker than a typical weld.

If the amount of current used exceeds the capability of the electrode, tungsten inclusions in the weld may result. Known as tungsten spitting, this can be identified with radiography and can be prevented by changing the type of electrode or increasing the electrode diameter. In addition, if the electrode is not well protected by the gas shield or the operator accidentally allows it to contact the molten metal, and it can become dirty or contaminated. This often causes the welding arc to become unstable, requiring that the electrode be ground with a diamond abrasive to remove the impurity. 

GTAW Quality

 

Tungsten Metals Manufacturer & Supplier: Chinatungsten Online - http://www.tungsten.com.cn
 Tel.: 86 592 5129696; Fax: 86 592 5129797
 Email: sales@chinatungsten.com
 Tungsten & Molybdenum Information Bank: http://i.chinatungsten.com
 Tungsten News & Tungsten Prices, 3G Version: http://3g.chinatungsten.com
 Molybdenum News & Molybdenum Price: http://news.molybdenum.com.cn