Experiments of Tungsten Copper Contacts Electrical Life

Tungsten copper contacts composition performance table of electrical life experiment

Experiment material

Density (g / cm³)

Hardness (HV10)

Conductivity (* 106S / m)

Gas content(*10-6)

W70Cu30

14-14.5

175-200

21-27

<35(O2+N2

W80Cu20

16.7-17

250-280

16-20

W90Cu10

15.2-15.6

210-250

18-23

Electrical erosion can be measured in a TDR-40A vacuum single-crystal furnace. Cathode material is tungsten copper contacts, a contact material, which has been processed into metallographic sample after polishing, anode material is pure tungsten (Φ = 2mm), they are placed in a vacuum furnace. Plus DC voltage of 8000V (in order to obtain a higher stability) between the anode and the cathode, so that the cathode can rise slowly with the speed of 0.2mm / min, let it close the anode until arc ignite between the anode and the cathode, arc every 30 times, using a precision (0.1mg) analytical balance to measure weight loss of a sample, total arc times is 300 times.

Employ 1000-B-type scanning electron microscope to scan morphology electrical erosion, and electron spectroscopy to analyze changes in the sample composition.

Tungsten copper contact

 

Tungsten Metals Manufacturer & Supplier: Chinatungsten Online - http://www.tungsten.com.cn
 Tel.: 86 592 5129696; Fax: 86 592 5129797
 Email: sales@chinatungsten.com
 Tungsten & Molybdenum Information Bank: http://i.chinatungsten.com
 Tungsten News & Tungsten Prices, 3G Version: http://3g.chinatungsten.com
 Molybdenum News & Molybdenum Price: http://news.molybdenum.com.cn